ASTM D1037 Test Methods for Wood-Base Fiber and Particle Panel Materials

Share:

ASTM D1037 - Standard Test Methods for Evaluating Properties of Wood-Base Fiber and Particle Panel Materials 


ASTM D1037 test methods cover small-specimen tests for wood-base fiber and particle panel materials that are made to provide:Data for comparing the mechanical and physical properties of various materials,

Data for determining the influence on the basic properties of such factors as raw material and processing variables, post-treatments of panels, and environmental influences, and

Data for manufacturing control, product research and development, and specification acceptance.

Test Scope: 

ASTM D1037 test methods cover the determination of the properties of wood-base fiber and particle panel materials that are produced as mat-formed panels such a particleboard, medium density fiberboard, hardboard, and oriented strand board.

ASTM D1037 Test Methods for Wood-Base Fiber and Particle Panel Materials

Applicable Products: 

Lumber and wood-base structural material


Test include in the ASTM D1037: 

Moisture Content and Conditioning Requirements

Accelerated Aging

Size, Physical Properties and Appearance of Panels

Static Bending

Tension Parallel to Surface

Tension Perpendicular to Surface

Compression Parallel to Surface

Fastener Holding Tests: 

   1. Lateral Nail Resistance

   2. Nail Withdrawal

   3. Nail-Head Pull-Through

   4. Direct Screw Withdrawal

Hardness

Hardness Modulus

Shear in the Plane of the Panel

Glue-Line Shear (Block Type)

Falling Ball Impact

Abrasion Resistance by the U.S. Navy Wear Tester

Moisture Tests:

 1, Water Absorption and Thickness Swelling

 2, Linear Expansion with Change in Moisture Content

Cupping and Twisting

Interlaminar Shear

Edgewise Shear

Compression-Shear

Modulus of Rupture

Tension Strength Parallel to Surface

Tension Strength Perpendicular to Surface

Water Absorption and Thickness Swelling

Moisture Content and Specific Gravity


ASTM D1037 Test Methods for Wood-Base Fiber and Particle Panel MaterialsASTM D1037 Test Methods for Wood-Base Fiber and Particle Panel Materials
Wood hardness testwood panel 3 points bending test


Related Standard

ASTM D143 Test Methods for Small Clear Specimens of Timber –

ASTM D143 – Standard Test Methods for Small Clear Specimens of Timber


ASTM D143 covers the determination of various strength and related properties of wood by testing small, clear specimens. These specimens are free of knots or other defects that might influence the test results. The standard includes a wide range of test methods for evaluating both mechanical and physical properties of wood.

ASTM D6109 Flexural Test of Unreinforced and Reinforced Plastic Lumber –

ASTM D6109 – Standard Test Methods for Flexural Properties of Unreinforced and Reinforced Plastic Lumber and Related Products


As Per ASTM D6109, "The test methods are suitable for determining the flexural properties for any solid or hollow manufactured plastic lumber product of square, rectangular, round, or other geometric cross section that shows viscoelastic behavior. The test specimens are whole "as manufactured" pieces without any altering or machining of surfaces beyond cutting to length. As such, this is a test method for evaluating the properties of plastic lumber as a product and not a material property test method. Flexural strength cannot be determined for those products that do not break or that do not fail in the extreme outer fiber."

Applicable Products: Plastic lumber products

ASTM D3500 Tension Test Methods for Structural Panels –

ASTM D3500 Standard Test Methods for Structural Panels in Tension

ASTMD3500 test methods cover the determination of the tensile properties of wood structural panels. To determine the tensile properties of wood structural panels in response to stresses acting in the plane of the panle. 


The Wood structural panels in use include plywood, oriented strand board and composites of veneer, and other wood-based layers.

EN 1382 Test methods for withdrawal strength of timber fasteners –

EN 1382 stipulated method to measure the maximum axial pull-out resistance of mechanical fasteners (nails, wood screws, staples) embedded in solid timber, glued laminated timber (glulam), LVL and CLT structural timber. It provides standardized raw data for structural timber engineering design and Eurocode compliance, focusing on solid structural timber rather than man-made wood composite panels (particleboard/MDF covered by EN 320 / ISO 27528). 

EN 320 Particleboard and fibreboard Screw Axial Withdrawal Test –

EN 320 Particleboards and fibreboards — Determination of resistance to axial withdrawal of screws is the official European test standard we fully support with our custom-built axial screw withdrawal testing machine.

This European norm defines a standardized laboratory test procedure to measure axial screw withdrawal resistance, also referred to as axial pull-out force, needed to pull calibrated standard screws out of particleboard, medium-density fibreboard (MDF) and high-density fibreboard (HDF) panels. Our universal testing machine paired with dedicated EN 320 screw pull-out fixtures delivers precise, repeatable force measurement that fully meets all specimen setup, axial loading and data recording rules laid out in EN 320.

ISO 27528 screw withdrawal resistance test of wood-based panels –

ISO 27528 defined to measure the maximum axial pull-out force required to extract screws from wood composite panels, covering two core test modes: face screw withdrawal and edge screw withdrawal. It serves as a global unified test method for evaluating the screw holding capacity of fibreboard, particleboard, OSB, plywood and other engineered wood panels with thickness ≥ 15 mm.

< Previous: ASTM D1004 Tear Resistance (Graves Tear) of Plastic Film and Sheeting

> Next: ASTM D1238 Polymer Melt Flow Rate Testing by Extrusion Plastometer

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.