ASTM B117: Standard Practice for Operating Salt Spray (Fog) Apparatus


Salt spray testing is one of the most critical methods for assessing surface treatment, coatings, and the corrosion resistance of metals, as well as ensuring product durability. All UnitedTest strictly adheres to ASTM B117, which is the globally recognized standard for salt spray testing. Standardized tests are conducted in a controlled environment to determine the corrosion resistance of materials, and it is commonly used in the automotive, aerospace, and manufacturing industries.With the help of ASTM standards, manufacturers like us provide accurate and stable test results, enabling our clients to improve product quality, extend service life, and ensure compliance with industry standards.


ASTM B117 provides standard practice for environmental and engineering services. The ASTM B117 is one of the most common standards for the salt spray test that defines certain parameters and specifications to perform the salt spray test in specific environmental conditions. 

This standard practice for operating salt spray apparatus must be followed by various industries, including –

Aerospace and aircraft

Automotive manufacturing

Construction and building materials

Infrastructure, such as water and sewer pipes

ASTM B117 is not restricted to salt spray operations only but also outlines the best practices for apparatus requirements, types and preparation of test specimens, temperature conditions, the timeline of the exposure period, etc.


Scope of Standard Practice

The scope of ASTM B117 standard practice in various industries regarding the operation and testing procedure of salt spray test. 

This practice describes the apparatus details, procedure, and conditions for creating and sustaining the salt spray (fog) test environment. It does not feature the test specimen shape or exposure times to be used for a specific product or the interpretation to be placed on the results.

The effect of salt spray on products:

The effects of product exposure to salt spray environment are divided into corrosion effects, electrical effects, and physical effects:

a),  Electrochemical corrosion and accelerated corrosion caused by other stresses;

b), Corrosion of acid/alkali solutions formed by ionization of salt in water.

c),  The settling and accumulation of salt spray on the surface and gaps of electronic products can lead to a decrease in electrical performance;

d),  The settling and accumulation of salt spray will generate new conductive layers, causing short circuits;

e),  Corrosion of electrical insulation materials.

f),  The settling and accumulation of salt spray can cause blockage and adhesion of mechanical components and moving parts of components;

g),  Electrolysis causes blistering or peeling of the protective paint layer.  

Salt spray test

Test objective: To assess the ability of materials to resist salt spray corrosion.

Test types: Neutral salt spray test NSS test, Acetic acid salt spray test AASS test, Copper accelerated acetic acid salt spray test CASS test, Alternating salt spray test, Advanced cyclic corrosion test

Severity level: solution concentration, pH value, salt spray deposition, duration

Evaluation methods: corrosion characteristics, corrosion area, weight changes, experience

Salt spray test type

(1) The neutral salt spray test (NSS test) is one of the earliest and most widely used accelerated corrosion testing methods. It uses 5% sodium chloride saline solution, and the solution PH value is adjusted in the neutral range (6-7) as the solution for spray. The experimental temperature is set at 35 ℃, and the settling rate of salt spray is required to be between 1-2ml/80cm2. h. Generally applicable to metals and their alloys, metal coatings (anodic or cathodic), conversion coatings, anodic oxide coatings, and organic coatings on metal substrates.

(2) The acetic acid salt spray test (AASS test) was developed based on the neutral salt spray test. It involves adding some glacial acetic acid to a 5% sodium chloride solution to lower the pH value of the solution to around 3, causing the solution to become acidic. The resulting salt spray also changes from neutral to acidic. Its corrosion rate is about three times faster than the NSS test.    

(3) The Copper Accelerated Acetic Acid Salt Spray Test (CASS Test) is a recently developed rapid salt spray corrosion test abroad. The test temperature is 50 ℃, and a small amount of copper salt - copper chloride - is added to the salt solution to strongly induce corrosion. Its corrosion rate is approximately 8 times that of the NSS test. Suitable for copper nickel chromium decorative coatings, nickel chromium decorative coatings, and anodized aluminum coatings.    

(4) The alternating salt spray test is a comprehensive salt spray test, which is actually a neutral salt spray test plus a constant humidity and heat test. It is mainly used for cavity type whole machine products. Through the infiltration of humid environment, salt spray corrosion not only occurs on the surface of the product, but also inside the product. It alternately converts the product between salt spray and humid and hot environments, and finally assesses whether the electrical and mechanical properties of the entire product have changed.



Related Standard

ASTM G155 Xenon Arc Lamp Test for Exposure of Materials Metals & Alloys –

ASTM G155: Standard Practice for Operating Xenon Arc Lamp Apparatus for Exposure of Materials


The ASTM G155 test apparatus exposes specimens to light, heat, and optionally moisture, often to attempt to replicate specimen property changes observed in outdoor and indoor end-use environments. Exposures are not intended to simulate the deterioration caused by localized weather phenomena, such as atmospheric pollution, biological attack, and saltwater exposure.


< Previous: ASTM A1064 Tension, Bend, Shear test for Steel Wire and Welded Wire Reinforcement, Plain and Deformed

> Next: ASTM B557 Aluminum and Magnesium Alloy Tension Testing

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.