Home >> Application >> By Standard >> ASTM >> ASTM D >> ASTM D4255 Rail Shear Test In-Plane of Polymer Matrix Composite Materials

ASTM D4255 Rail Shear Test In-Plane of Polymer Matrix Composite Materials

Share:

ASTM D4255 Standard Test Method for In-Plane Shear Properties of Polymer Matrix Composite Materials by the Rail Shear Method


ASTM D4255 is a test method for testing the in-plane shear properties of high-modulus fiber-reinforced composite materials. The method is divided into two procedures. Procedure A tests laminates clamped between two pairs of loading rails. When loaded in tension the rails introduce shear forces in the specimen. In Procedure B, laminates clamped on opposite edges with a tensile or compressive force applied to a third pair of rails in the center are tested. 


Properties that may be measured by this test method include:

 In-plane shear stress versus engineering shear strain response,

 In-plane shear chord modulus of elasticity,

 Offset shear stress, and Maximum in-plane shear stress. 

ASTM D4255 Rail Shear Test In-Plane of Polymer Matrix Composite Materials

In cases in which the engineering shear strain at failure is greater than 5 %, the shear stress corresponding to 5 % engineering shear strain should be reported.


ASTM D4255 Rail Shear Test In-Plane of Polymer Matrix Composite Materials


< Previous: ASTM D4161 Coupling leakage hydrostatic pressure test for GRP fiberglass Pipe Joints seals

> Next: ASTM D4329 Ultraviolet (UV) Lamp Exposure of Plastics

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.