SANS 6282 Twisting torsion test for hard-drawn and high-tensile strength conductors SANS 182
It's follow the ISO 7800, 7801, 7802 test as below:
ISO 7800:2003 specifies a method for determining the ability of metallic wire of diameter or characteristic dimension 0,1 mm to 10 mm inclusive to undergo plastic deformation during simple torsion in one direction.
ISO 7802: Metallic materials -- Wire -- Wrapping test equipment
ISO 7801: GOST 1579 Metal Wire Reverse Bend Testing Machine
A test piece of wire is twisted a specified number of turns through 360° around its own axis in one direction, and then a specified number of turns through 360° in the opposite direction. The wire specimen be twisted about the longitudinal axis until it fails. Upon failure, the number of turns should be recorded.

UnitedTest conductors wire testing machine, include the torsion, reverse bending, wrapping test of wires.