Climbing Drum Peel test for Adhesives - ASTM D1781
Date:2018-07-18 Source:United Test Views:100

This procedure is useful for the determination of the peel resistance of adhesive bonds adhering a relatively flexible and adhering rigid; and the relatively flexible coating of a sandwich structure and its nucleus, to the test under the specified conditions.

This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.