EN 13888‑2 flexural and compressive strength test of Grouts for ceramic tiles
Date:2025-07-26 Source:United Test Views:100

EN 13888-2: Grouts for ceramic tiles - Part 2: Test methods


EN 13888-2 standard specifies the methods for determining characteristics for grouts used in internal and external installation of ceramic tiles.

Test methods: 

-   Determination of flexural and compressive strength (9.1);

-   Determination of water absorption (9.2);

-   Determination of shrinkage (9.3);

-   Determination of resistance to abrasion (9.4);

-   Determination of chemical resistance (9.5).