ISO 9969 Thermoplastics pipes of ring stiffness test equipment
Date:2025-05-22 Source:United Test Views:100

ISO 9969 specifies a test method for determining the ring stiffness of thermoplastics pipes having a circular cross section. 

ISO 9969 requires that at least three samples are taken from the same pipe and labeled A, B and C. These samples are then compressed to at least 3% of the Inner Diameter and ring stiffness calculated for each sample. The ring stiffness is calculated as an average of these calculations. 


The initial ring stiffness or ring stiffness to ISO 9969 or ASTM D2412 characterizes the resistance of a pipe section to radial compressive forces. The measurement occurs at low deformations of 3%.   


Get the product for ISO 9969 at here: ISO 9969 Thermoplastics pipes of ring stiffness test equipment

Ring stiffness.jpg

Related products
Contact

Email:
export@unitedtest.com
unitedtest@hotmail.com
Tel:
+86-10-57055071
+86-13911165373

MS Teams: 
unitedtest@hotmail.com

WhatsApp:
+86 13911165373

WeChat:
UnitedTest-V1 

X