ISO 4589-2 Plastics — Determination of burning behaviour by oxygen index Part 2: Ambient-temperature test
Date:2024-11-01 Source:United Test Views:100

ISO 4589-2:2017 specifies methods for determining the minimum volume fraction of oxygen, in admixture with nitrogen, that will support combustion of small vertical test specimens under specified test conditions. The results are defined as oxygen index (OI) values.


UNTIEDTEST YZS series oxygen index tester is designed for this standard test. 


Methods are provided for testing materials that are self-supporting in the form of vertical bars or sheets up to 10,5 mm thick. These methods are suitable for solid, laminated or cellular materials characterized by an apparent density 100 kg/m3 or greater. The methods might also be applicable to some cellular materials having an apparent density of less than 100 kg/m3. A method is provided for testing flexible sheets or film materials while supported vertically.


For comparative purposes, a procedure is provided for determining whether or not the OI of a material lies above some specified minimum value.


Related products
Contact

Email:
export@unitedtest.com
unitedtest@hotmail.com
Tel:
+86-10-57055071
+86-13911165373

MS Teams: 
unitedtest@hotmail.com

WhatsApp:
+86 13911165373

WeChat:
UnitedTest-V1 

X