ISO 13003 Fatigue dynamic test, Fibre-reinforced plastics — Determination of fatigue properties under cyclic loading
Date:2025-05-04 Source:United Test Views:100

ISO 13003 Fatigue dynamic test, Fibre-reinforced plastics — Determination of fatigue properties under cyclic loading

ISO 13003 defines the general procedures for fatigue testing of fibre-reinforced plastic composites under cyclic loading condition.

It addresses tension-tension fatigue of fiber reinforced plastic composites with Axial tensile fatigue test or flexural bend test. UnitedTest Fatigue testing machine, 100KN, 50KN etc., The plastic fatigue testers that we build can be configured for fatigue testing of plastic.

Systems that fatigue test plastic such as the ones from UnitedTest load the plastic specimen with cyclic constant amplitude load while also making accurate measurements of strain and stress.

cd210f9c1ac7d234aee313c9920fdf81.png

29884955a9ce42eefea04cc54c74d3e0.png

Related products
Contact

Email:
export@unitedtest.com
unitedtest@hotmail.com
Tel:
+86-10-57055071
+86-13911165373

MS Teams: 
unitedtest@hotmail.com

WhatsApp:
+86 13911165373

WeChat:
UnitedTest-V1 

X