ISO 7539-7 slow strain rate testing metals and alloys stress corrosion testing machine. Slow Strain Rate Stress Corrosion Cracking Test
ISO 7539-7:2005 covers procedures for conducting slow strain rate tests for investigating susceptibility of a metal to stress corrosion cracking, including hydrogen-induced failure. The term "metal" as used in this part of ISO 7539 includes alloys.
Slow strain rate tests are adaptable for testing a wide variety of product forms, including plate, rod, wire, sheet and tubes, as well as composites of these and parts joined by welding. Notched specimens may be used, as well as initially plain specimens.
The principal advantage of the test is the rapidity with which susceptibility to stress corrosion cracking of a particular metal/environment combination can be assessed.
Application scope
The ISO7539-7:2005 standard is applicable to various metal materials and alloys, including but not limited to ferroalloys, stainless steel, aluminum alloys, titanium alloys, etc. Through this testing method, engineers and researchers can better understand the characteristics of materials, optimize material selection and process parameters, and improve product quality and reliability.
Test significance
Evaluating corrosion resistance: Through slow strain rate stress corrosion testing, the corrosion resistance of alloys under different environmental conditions can be evaluated, providing important basis for material selection.
Predicting cracking risk: This standard can be used to predict the stress corrosion cracking risk of alloys in practical engineering applications, providing a basis for design, production, and use.
Optimizing material selection: By understanding the performance of alloys in specific stress corrosion environments, material selection can be optimized to improve the overall performance of products.
Improving engineering safety: By following this standard for testing, it can be ensured that the alloy has sufficient resistance to crack propagation under actual working conditions, thereby ensuring the safe operation of engineering structures.

Practical application
The ISO7539-7:2005 standard has a wide range of applications in fields such as aerospace, petrochemicals, and nuclear industry. These fields have high requirements for the corrosion resistance and reliability of materials, so the application of this standard in these fields is particularly important.
Beijing United Test Co.,Ltd. export@unitedtest.com offer the testing equipment of ISO 7539-7 slow strain rate testing metals and alloys stress corrosion testing machine, Slow Strain Rate Stress Corrosion Cracking Test. Contact us now : export@unitedtest.com, unitedtest@hotmail.com