Your current locationHome > Products > Hardness tester > Vickers hardness tester
Products
HV Series Vickers Hardness Tester (Durometer)

All Vickers ranges use a 136° pyramidal diamond indenter that forms a square indent.

1, HV series Vickers Hardness Tester made with a unique and precision design in the field of mechanics, optics and light source is able to produce a clearer indentation and hence a more precise measurement.
2, Equipped with a 10* eyepiece for measurement;
3, Adopt cold light source, the using life of light source can reach 100000 hours
4, With LCD screen, customer can select HV/HK or change the hardness value by the option menu, The testing result (via the internal data processing) is shown on screen.
5, “Z” type has an automatically turning turret to change the object lens and indenter;
6, With a special thread interface, the tester can be linked with CCD video measuring system or LCD screen measuring system;
Model HV-5/HV-5Z HV-10/HV-10Z HV-30/HV-30Z HV-50/HV-50Z
Test force N 2.942, 4.903, 9.807, 19.61, 24.52, 29.42, 49.03 2.942, 4.903, 9.807, 29.42, 49.03, 98.07 9.807, 29.42, 49.03, 98.07, 196.1, 294.2 9.807, 49.03, 98.07, 196.1, 294.2, 490.3
Kg 0.3, 0.5, 1, 2, 3, 5 0.3, 0.5, 1, 3, 5, 10 1, 3, 5, 10, 20, 30 1, 5, 10, 20, 30, 50
Force loading mode Automatic loading, holding and unlaoding
Holding time 0-60S
Amplification of microscope 100*, 200* 200*,100* 100*
Min. measuring resolution rate 0.125μm(200*), 0.250μm(100*),
Testing field 8HV0.3~2900HV10
Lens/indenter switch mode HV series : Manually
HV-Z series: Motorized
Dimension of XY table 100*100mm ***
Moving range of XY table 25*25mm ***
Max. height of test sample 160mm
Max.width of test sample 135mm
Light source Cold light source
Objectives 10*, 20*, 40* according customer requirement
Power AC 220V, 50/60HZ
Dimensions 520*190*650mm
Net Weight 40Kg
Standard Accessories XY-stage test table, thin specimen test table, fine wire test table, Fork-shaped test table Large test table,
V shape test table
10* digital micro lens, adjustable screw, vikers hardness block, manual etc.
XY-stage test table,
thin specimen test table,
fine wire test table,
Fork-shaped test table
Large test table,
V shape test table

10* digital micro lens,
adjustable screw,
vikers hardness block,
manual etc.
ASTM E384 “Standard Test Method for Microindentation Hardness of Materials”

ISO 6507 “Metallic materials -- Vickers hardness test”

Your email address
Your message

contact
Email:
export@unitedtest.com
unitedtest@hotmail.com
Tel:
+86-10-57055071
+86-13911165373
SKYPE:unitedtest08
WhatsApp:
+86 13911165373
X