Metal wire wrapping testing machine

NCR series metallic materials wire wrapping testing machine used for determining the ability of wire of diameter or thickness 0,1 to 10 mm inclusive to undergo plastic deformation during wrapping. The test consists of winding a wire to a specified number of turns around a mandrel of the diameter specified in the relevant standard to form a closely wrapped helix. It may also include a specified sequence of windings and unwindings, or even rewindings.

Standard: ISO 7802: Metallic materials -- Wire -- Wrapping test.
Model NCR-6 NCR-10
Sample diameter 0.1-6mm 0.1-10mm
Wrapping speed 15, 20, 60R/min
Dimensions 700*500*1150mm
Weight 210Kg 230Kg
No information
ISO 7802: Metallic materials -- Wire -- Wrapping test.
Your email address
Your message

contact
Email:
export@unitedtest.com
unitedtest@hotmail.com
Tel:
+86-10-57055071
+86-13911165373
SKYPE:unitedtest08
WhatsApp:
+86 13911165373
X